Author(s): Mahendra Kumar Gupta, Sonia Nayak, Amit Ku. Kachhawaha
Abstract The defects of the centrifugally cast samples was decrease the strength and quality of product. Randomly design the experiments has been used, to analyses the influence of process parameters on the defects during centrifugal casting of aluminum alloy. Tests carried out on Eight design of experiment characterized by different variation of Speed Temperature and Type of cooling on aluminum alloy that solidify and analysis the defects of shrinkage and blow holes produce during cooling. The process of centrifugal casting has to be optimizing their quality.